A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: SU-8 spinning problems
SU-8 spinning problems
2002-03-15
Glen Landry
2002-03-15
[email protected]
2002-03-15
CLIF HAMEL
2002-03-15
Vic Kley
2002-03-15
Henry Yang
2002-03-15
[email protected]
wafer level vacuum packaging
2002-03-15
Krishna Kashyap
2002-03-15
CLIF HAMEL
SU-8 spinning problems
CLIF HAMEL
2002-03-15
Yes, 200 rpm per second, not thousands.  A slow acceleration helps the
material spread a little more evenly.

Clif

Clifford J. Hamel
Suss Microtec Applications Engineer
(802) 244-5181, ext 297

>>> [email protected] 03/15/02 02:32PM >>>
> "200 rpm per second" ? Cliff???
>
> 200 rpm means 200 revolutions per minute.  Are you suggesting an
> acceleration or is it just a mistake?

When you program a newer model of spinner,
you can set the acceleration in addition to the rotational speed.
For example, an MTI Flexifab take takes the acceleration in krpm/s.

        --Kirt Williams Agilent Technologies
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
MEMS Technology Review