MEMSnet Home: MEMS-Talk: How to get 2" Si wafer and etch 45 degree V-groove?
How to get 2" Si wafer and etch 45 degree V-groove?
2002-03-18
lib zhou
How to get 2" Si wafer and etch 45 degree V-groove?
2002-03-19
Kenneth Smith
How to get 2" Si wafer and etch 45 degree V-groove?
Kenneth Smith
2002-03-19
Lib,

Contact me on the 2" .
On the the material that you are using that you had expected the 45
degree and obtained the 54.7 degree was clearly not Off cut at 9.7
degree as this Off cut WILL obtain the 45 degree V-groove. We have
supplied this material to other users and have not had incident of poor
yields and obtained the 45 degree V groove. It appears that your
material is cut ON orientation.

Regards,
Ken Smith


lib zhou wrote:

> Hi,Dear All:
>
> I am interested to know if anyone can send me some information which company
> can still sell high quality 2" single-crystal silicon wafer. by the way, I
have an another
> question related to (100) Si anisotropic etch by KOH, how can get a 45 (or
135)degree

  bevel plane at the end of a V-groove, this angle refer to the inclination of
the end bevel

plane to the V-groove axes line (or bottom line). I think the method cuting
(100) silicon at

 9.7 degree angle can only get the bevel plane have a 45degree to Si surface,
the angle

 between the bevel plane and the V-groove bottom line is still -54.7 degree.
>
>
> Thanks ahead and best regards,
>
> Lib Zhou
> Yahoo! Sports - live college hoops coverage
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.mems-exchange.org/
>
>


--


Kmbh Associates
47 Rocket Circle
Rancho Cordova, CA 95742  U  S  A
510-714-5055 Efax- 510 217 4421 or 561 658 6136

High Purity Float Zone and Specialty CZ Silicon  for Power, IR and
Mirror Optics, Optoelectronics, MEMS, SOI, and other Semiconductor
applications. Service in SOI, Polishing SSP and DSP.
Quartz, Glass, Pyrex and Borofloat Wafer Supply. Anodic Bonding. SOG, SOS.

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
MEMStaff Inc.
University Wafer
Process Variations in Microsystems Manufacturing