MEMSnet Home: MEMS-Talk: wafer level vacuum packaging
wafer level vacuum packaging
2002-03-18
Mike Mattes
2002-03-18
RobDavis
Hexsil process
2002-03-18
Sun Yu
cantilevers
2002-03-19
Sun Yu
2002-03-20
[email protected]
2002-03-20
Vic Kley
2002-03-20
Krishna Kashyap
2002-03-19
shay kaplan
Stero lithography service.
2002-03-21
il-seok Son
wafer level vacuum packaging
Krishna Kashyap
2002-03-20
is it vacuum packaging?
is so is it under 100 millitorr?
for how long can the vacuum stay?

krishna

-----Original Message-----
From: [email protected] [mailto:[email protected]]On
Behalf Of RobDavis
Sent: Monday, March 18, 2002 10:32 AM
To: [email protected]
Subject: RE: [mems-talk] wafer level vacuum packaging


We are in the prototype stages of a total silicon carbide package and chip
for extreme service.  Silicon carbide is good as a semiconductor over 600C
and our resistors good to 1000 C using high temperature contacts.  The
package is made from polycrystalline silicon carbide wafers and sealing is
done in a controlled atmosphere furnace.

Rob

-----Original Message-----
From: [email protected] [mailto:[email protected]]On
Behalf Of Mike Mattes
Sent: Monday, March 18, 2002 7:30 AM
To: [email protected]
Subject: Re: [mems-talk] wafer level vacuum packaging


Has any company actually commercialized a product using wafer level
packaging?

Best Regards,
Mike Mattes
Medtronic, Inc.



>>> [email protected] 03/15/02 04:56PM >>>
I am interested to know if anyone can send me information regarding
techniques, companies, research etc. in this area.

Krishna Kashyap
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
University Wafer
Addison Engineering
MEMStaff Inc.