MEMSnet Home: MEMS-Talk: Need Information about simple mask making
Need Information about simple mask making
2002-03-27
Richard Chen
2002-03-27
Mighty Platypus
2002-03-27
[email protected]
2002-03-28
Craig McGray
Need Information about simple mask making
Mighty Platypus
2002-03-27
Hi Richard,
We use CCI Graphics, out of Gardena for Printshop masks. They can go down
to about 30-40um, and they'll make a 5x5 glass mask for about $65. You can
reach them at 310-515-0922.

Jesse Fowler
  UCLA/MAE Dept., 420 Westwood Plaza, Room 37-129, ENGR IV
  Los Angeles, CA 90095-1597 | (310)825-3977
"Battery is safe if not provoked." -- _Batteries in a Portable World_

On Wed, 27 Mar 2002, Richard Chen wrote:

> Hi all,
> I am lookin for a way of making the mask from the printer. Can anybody
> suggest me where I can get this service near the L.A. area? Thanks!
>
> Richard Chen
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Addison Engineering
Harrick Plasma, Inc.
MEMS Technology Review