photosensitive polyimides
Mac McReynolds
2002-03-28
Check archmicro.com.  I think they took over the Probimide series originally
from Ciba Geigy/Merck venture

Mac McReynolds
R&D Manager
Caliper Technologies Corp.
605 Fairchild Drive
Mountain View, CA 94043-2234
Tel:  650-623-0710
Fax:  650-623-0521

> ----------
> From:         Balaji Lakshminarayanan
> Reply To:     [email protected]
> Sent:         Wednesday, March 27, 2002 9:02 PM
> To:   [email protected]
> Subject:      [mems-talk] photosensitive polyimides
>
> Hi,
>
> Can anyone tell me companies that sell photosensitive polyimides. I am
> using it as a dielectric for variable capacitors. I searched the web and
> found clariant (their PIMEL series) sells the same, but they told us the
> quantities they ideally sell is difficult for educational institution to
> handle.
>
> Your help is greatly appreciated
>
> regards
>
> bala
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
Nano-Master, Inc.