MEMSnet Home: MEMS-Talk: Etching through a silicon wafer
Etching through a silicon wafer
2002-04-09
Gao, Yuanfang (UMC-Student)
2002-04-10
[email protected]
2002-04-10
Michael D Martin
2002-04-22
il-seok Son
2002-04-12
BERAUER,FRANK (HP-Singapore,ex7)
Etching through a silicon wafer
Michael D Martin
2002-04-10
I have had problems with deadhesion of Ti/Pt in TMAH. That is the Pt
came off! I would not be surprised if Au behaves similarly, unless I had
a sputtering problem.

-Mike

>>> [email protected] 04/09/02 03:09PM >>>
Dear all,

I plan to use anisotropic wet etching to etch through holes in a
<100>silicon
wafer, using LPCVD silicon nitride as mask layer,
also there is a exposed Ti/Au layer(Ti act as a adhesion layer)
on top of silicon nitride.
My concern is:

1. Will Ti/Au layer resist the long time KOH etching?
2. If KOH doesn't work, will other etchants like TMAH do?
3. Will KOH etching damage the silicon nitride membrane?

Thank you very much!

Yuanfang Gao

University of Missouri
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk

Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Addison Engineering
Mentor Graphics Corporation