MEMSnet Home: MEMS-Talk: RE: Commercial DRIE services w/ SOI anti-footing option.
RE: Commercial DRIE services w/ SOI anti-footing option.
2002-04-12
Heaton, Monte
RE: Commercial DRIE services w/ SOI anti-footing option.
Heaton, Monte
2002-04-12
Hello Jennifer:

Innovative Micro Technology has the STS DRIE with the anti-footing option
and has extensive etching experience.  This and our other
capabilities/experience are described on our web site at www.imtmems.com
 .  Please call me directly if you would like to
inquire about our services.

Regards- Monte.

Monteith G. Heaton 
VP Marketing and Sales
Innovative Micro Technology
75 Robin Hill Road * Santa Barbara, CA  93117
Ph:  805-681-2852 * Fx:  805-967-2677
[email protected]   * www.imtmems.com

_________________________________________
"Your strategic partner for MEMS design and 6" wafer
manufacturing services with 0.355m photolithography,
30,000 sq. ft. fab, and non-CMOS materials flexibility,
including metals/magnetics."



-----Original Message-----
From:   Jennifer Scalf [mailto:[email protected]]

Sent:   Friday, April 12, 2002 1:11 PM
To:     [email protected] 
Subject:        [mems-talk] Commercial DRIE services w/ SOI anti-footing
option.

I am looking for commercial vendors of DRIE services-specifically, I am
looking for vendors whose DRIE machines are outfitted with the SOI
anti-footing capability (i.e. pulsed platen power).
I know for sure ISSYS and SNF do not have the anti-footing option.
Any leads would be appreciated.
Thank you very much,
J. Scalf


_________________________________________________________________
Join the world_s largest e-mail service with MSN Hotmail.
http://www.hotmail.com 
_______________________________________________
mailing list: to unsubscribe or change your list options, visit
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
  Hosted by the
MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/ 

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Addison Engineering
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing