PDMS pillar shape
Bo He
2002-05-16
Dear All:

         I am working on making pillar arrays by PDMS. But when I pull
out PDMS from SU8 mold, I found most pillars were deformed (bent). The
reason I am thinking about is that the cavity on SU8 mold has positive
slope hence PDMS pillar has negative slope. The the top of PDMS pillar,
which is in contact with the bottom of the cavity on SU8 mold, is larger
then the bottom, so it's deformed or bent during pulling out. Is there
anyway to solve the problem? Any suggestion is highly appreciated.

Bo

------------------------------------------------------------------------

Chat with friends online, try MSN Messenger: Click Here

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation