A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: HF and photoresist mask
HF and photoresist mask
2002-05-30
Jing Liu
2002-05-30
Mighty Platypus
2002-05-30
Bill Moffat
2002-05-30
Henry Yang
2002-05-30
[email protected]
2002-06-03
Soojin Oh
2002-05-31
Jing Liu
2002-05-31
Mighty Platypus
metal-glass bonding and debonding
2002-06-03
carlton watson
2002-05-31
Greg Miller
2002-05-31
Bill Moffat
2002-05-31
Bill Moffat
2002-05-31
Bill Moffat
2002-05-31
Jing Liu
2002-05-31
Roger Shile
HF and photoresist mask
Bill Moffat
2002-05-30
The secret in this case is definitely vacuum vapor prime.  An etch I used to
do on 17,000 Angstroms of thermal Silicon Dioxide using a spray HMDS as the
adhesion promoter seemed dependent on any factor that could affect it.  Tests
done on vacuum primed wafers that had been sitting in the open for 7 days
showed no problems.  Contact me for more details.  Bill Moffat

-----Original Message-----
From: Jing Liu [mailto:[email protected]]
Sent: Thursday, May 30, 2002 12:34 PM
To: [email protected]
Subject: [mems-talk] HF and photoresist mask


To who may concern,

I want to mask HF etching with photoresist. Just now, somebody suggest me
that
for the same thickness of oxide I will etch. The photoresist could stand
buffered HF, but for concentrated HF, it will not. Is it exactly the case?
Could I be able to find some reference?

BTW, we have Shipley 1813, AZ 5214, Az 9245 in the lab. Does anyone have some
date of how fast they will etched in HF?

Thanks,

Jing
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
Mentor Graphics Corporation