Dear colleagues,

>I have a problem. I have to etch a thin film (200 angstrom) of Gold over a
>film of Nickel but I DON'T have to remove Nickel.

How can I do this?

Thank you
Luciano Scaltrito

--------------------------------------------------------------------------------
--------
                ~ The truth is out there ~
Ing. Luciano Scaltrito
Dipartimento di Fisica
Politecnico di Torino
C.so Duca degli Abruzzi, 24
10129 Torino, Italy
tel +39 011 564.7305/564.4160
fax +39 011 564.7399
E-mail : [email protected]
http://www.polito.it/centri/laborato/limadel/film/index.html
--------------------------------------------------------------------------------
-------
-

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
University Wafer
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing