anisotrophic wet etchant for GaAs
2002-07-23
HeeTaek Yi
2002-07-24
Parshant Kumar
2002-07-23
[email protected]
2002-07-24
oray orkun cellek
anisotrophic wet etchant for GaAs
[email protected]
2002-07-23
We produce an rie system that can give the anisotropic profile you are
looking for but as far as I know there is no wet etch that will give similar
results due to the crystal orientation of GaAs. Bob Henderson

reply