Hi, everyone,

I am working with AZ1518 on flat panel display. Could anyone give me some
suggestion what kind of
hard bake temperature I should use? I just want to bake 1.6 um resist hard
enough to resist wet
etching.

Thanks.


Yun Li
KWB405, Thin Films Lab
Micro and Nano Structures
One Research Circle, Niskayuna, NY 12309
GE Global Research Center

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Addison Engineering
University Wafer
Tanner EDA by Mentor Graphics