[email protected] will do mylar photoplots cheaply - the resolution is about
25 microns (1 mil.)  Not as cheap as a laser printer, but very high quality.
The most cost effective way is to put many plots on a single drawing, plot
out a big drawing, and cut it up.

The only problem is that you need to send them files in gerber format.  They
do conversions from dxf, but that costs $125.
There are several software programs that will convert from dxf to gerber.  I
haven't found a free one yet.  However, at
http://www.innoveda.com/default.asp you can download a demo version of
CAM350, which will allow you to do conversions from dxf to gbr - the demo
version limits the size and complexity of the mask.  There may be other
options for conversion out there.  (If anyone knows of an open source file
or software library that does these conversions, I'd love to hear about it!)

Good luck!



David Nemeth
Senior Process Engineer
Sophia Wireless, Inc.
14225-C Sullyfield Circle
Chantilly, VA
Ph: (703) 961-9573 x206
Fax:(703) 961-9576

-----Original Message-----
From: [email protected] [mailto:[email protected]]On
Behalf Of Michael Wulf
Sent: Tuesday, August 20, 2002 1:21 PM
To: [email protected]
Subject: [mems-talk] Laser printer masks


Hi,

i need some cheap masks; the easiest solution we found is using a
laser-printer on overhead foiles. the structure size i can reach with this
is so far limited to be 200microns.

does anybody have experinece how to make structures smaller (without
spending money on a mask) and what brands (models) of transparencies and
printers might be good ? (i aim at a factor of 2 to 4 in structure size)

does anybody know a place where you can buy such really cheap masks with
even better resolution ?


thanks already,

mike
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
The Branford Group
Tanner EDA by Mentor Graphics