polymer materials
Nickel etchant
2002-09-10
Eric Sanjuan
2002-09-11
Adrian Stoian
2002-09-11
Rivas, Isabel
polymer materials
Rivas, Isabel
2002-09-11
Hello Adrian,

The polyimides have high chemical resistance, high thermal stability with a
glass transition temperature, Tg > 300º C and they are very strong.
I don't know if this information can help you.

Best regards,

Isabel Rivas Guerrero
[email protected]
> CEIT, Microelectronic section.
> Paseo de Manuel Lardizábal, 15.
> 20018 San Sebastián, Spain



-----Original Message-----
From: Adrian Stoian [mailto:[email protected]]
Sent: 11 September 2002 10:11
To: [email protected]
Subject: [mems-talk] polymer materials



        Hi,

    I am interested if there is anyody that have more information about the=
 polymeric materials with chemo-mechanical properties. I am also interest t=
o study these materials for an artificial muscle.  I would like to apply fo=
r a PhD grant in this area of research.

       Greetings,
=20
       Adrian

--=20
This message has been scanned for viruses and
dangerous content by MailScanner, and is
believed to be clean.

_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Nano-Master, Inc.
MEMStaff Inc.
The Branford Group