MEMSnet Home: MEMS-Talk: poly-Si Deep Trench Etch
poly-Si Deep Trench Etch
2002-09-11
Sunghon Chi
poly-Si Deep Trench Etch
Sunghon Chi
2002-09-11
Hi~

I'm trying to make poly-Si deep trench with LAM9400 or AMAT MxP poly etcher.
Mininum feature size is 3um and depth is 20um.
And vertical profile is needed; over 89¢ª
And hard mask for poly etch is PETEOS oxide of 1.5um.
Oxide etch will be done with TEL IEM oxide etcher.
I'll start with Cl2+O2 gas chemistry for poly etch.

If there is anybody who have done similar experience,
please give me comment.

Best Regard,
Sunghon Chi

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
MEMS Technology Review
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation