MEMSnet Home: MEMS-Talk: Si/SiO2 KOH etching selectivity
Si/SiO2 KOH etching selectivity
2002-09-16
Yanjun(David) Tang
2002-09-16
bille@npphotonics (Bill Eaton)
2002-09-17
Antje Wiegand (2 parts)
Si/SiO2 KOH etching selectivity
Antje Wiegand
2002-09-17
Hi Yanjun(David) Tang,

Take Tetramethylammoniumhydroxide/2-Propanol (3+1mixture) at 80 ° C  instead of
KOH.

Best regards
Antje Wiegand


"Yanjun(David) Tang" schrieb:

> Hi, MEMS folks
>      I've been working on releasing SiO2 cantilever beams from Si with KOH wet
etching. SiO2 beams was attached to Si layer at one side. The temperature is 80
degree-C and stirring is 220RPM. The etching time is about 15mins. By
caculation, only 15um Si layer needs to be etched away to release cantilever
beam. I didn't get satisfactory etching selectivity on Si/SiO2 etching rate.
SiO2 beams began to be etched even before Si was cleaned. The resulted
cantilever beam wasn't integrated. Do you have some suggestions about how to
increase the etching selectivity or any ideas about releasing SiO2 cantilever
beams from Si. Thanks.
>
> Best regards
>
> Yanjun(David) Tang
>
> Graduate student
> Institute for Micromanufacturing
> Louisiana Tech University
>
> 1401 Tech Farm Rd. Apt. #238, Ruston, LA 71270, USA
> Email: [email protected]
>           [email protected]
>
> Tel: 1-318-255-5133
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/
antje.vcf (text/x-vcard, 247 bytes)
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.