MEMSnet Home: MEMS-Talk: How to clean Si wafer with Cr/Au before anodic bonding
How to clean Si wafer with Cr/Au before anodic bonding
2002-09-28
Phyllis Yuen
How to clean Si wafer with Cr/Au before anodic bonding
Phyllis Yuen
2002-09-28
I would like to bond Si and pyrex wafer together by anodic bonding.  My Si wafer
has some trenches which the bottom is covered by a 200A Cr/ 500A Au.  How can I
clean this Si wafer before anodic bonding?  Can I do RCA SC1 clean
(water+H2O2+Ammonia solution) to remove organic contaminations, without the RCA
SC2 clean (water+H2O2+HCl), which remove the metallic contaminations?

Thank you very much for your help!

Phyllis

UC Davis



---------------------------------
Do you Yahoo!?
New DSL Internet Access from SBC & Yahoo!
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
The Branford Group
MEMS Technology Review
Process Variations in Microsystems Manufacturing