Hi,

how can I etch gold slowly (~100 nm/min)?
Can I slow etching by diluting etch-solution (4g KI / 1g I2 / 40ml H2O),
which etches 500-1000 nm/min?
If so, does the etch-rate reduce linearly with consentration of KI and I2?


-Sampo Tuukkanen, University of Jyväskylä, FINLAND



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
MEMStaff Inc.
The Branford Group
Process Variations in Microsystems Manufacturing