MEMSnet Home: MEMS-Talk: removing AZ4562 photoresist after exposure to CF4 plasma
removing AZ4562 photoresist after exposure to CF4 plasma
2002-10-29
Michael D Martin
removing AZ4562 photoresist after exposure to CF4 plasma
Michael D Martin
2002-10-29
There's a real handy product called Nanostrip, a mixture of buffered
acids, that is great for removing any type of resist. It will not damage
polyimide. You can get it here:
http://www.cyantek.com/catalog/cleansol.htm .

-Mike

>>> [email protected] 10/29/02 03:14AM >>>
Dear fellows,

I have a 6 um thick layer of AZ4562 photoresist, which was used to
pattern a 1 um thick Si3N4 layer, etched in CF4 plasma for about 35
min. The resist is cured for 45 min at 110 degC. There must be
something bad going on with the top of the resist layer, since it is
not removable in Aceton (which works fine, usually, with that kind of
resist). A O2 plasma strip for 10 min (1000W, 100 mTorr) after the
SiN etch doesn't help either. I can't etch too long in O2 plasma
since I have a polyimide layer on my wafer which should at least not
been underetched.

Any guess on how to remove AZ4562 after CF4 exposure? Without
attacking other materials (polyimide)?

I'm very grateful for any help or contact,

Joachim Oberhammer.
--
------------------------------------------------------------------------------
Joachim Oberhammer, Dipl.-Ing.

Royal Institute of Technology (KTH)   Phone:    +46/(0)8 790 6250
Dep. of Signals, Sensors and Systems  Fax:      +46/(0)8 10 0858
Microsystem Technology (MST)          Mobile:   +46/(0)70 692 1858
                                       e-mail:
[email protected]
Osquldas vSg 10                       homepage:
http://www.s3.kth.se/mst/
SE-100 44 Stockholm, Sweden

_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://www.memsnet.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing