Bonding Si to Si
2002-10-31
Josef Kouba
2002-11-01
CLIF HAMEL
2002-11-01
Luesebrink Helge
2002-11-01
Jeff Birkmeyer
2002-11-01
Kenneth Smith
2002-11-04
Josef Kouba
Bonding material impervious to KOH bath
2002-11-02
[email protected]
2002-11-04
Atzmon Ofri
Bonding Si to Si
Luesebrink Helge
2002-11-01
Josef,


You can find technical papers and application notes on wafer bonding at
http://www.evgroup.com/papers/memspapers.htm

Best regards,
Helge


 -----Original Message-----
From:   Josef Kouba [mailto:[email protected]]
Sent:   Thursday, October 31, 2002 2:18 PM
To:     'MEMS talk'
Subject:        [mems-talk] Bonding Si to Si

Hi all MEMS talk members,

can anybody give me some advise how to bond two silicon wafers together?
Do I need some special wafers for it or can I use common wafers? I would
also appreciate any reliable and good information source about this
problem.

Thanks for your help

Best Regards

Josef Kouba
Louisiana State University
Center foot Advanced Microstructures & Devices
6980 Jefferson Hwy.
Baton Rouge, LA 70806, USA
(225) 578-9371 - Tel.
(225) 578-6954 - Fax.


_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://www.memsnet.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
Tanner EDA by Mentor Graphics