2002-10-31
Josef Kouba
2002-11-01
CLIF HAMEL
2002-11-01
Luesebrink Helge
2002-11-01
Jeff Birkmeyer
2002-11-01
Kenneth Smith
2002-11-04
Josef Kouba
Bonding material impervious to KOH bath
2002-11-02
[email protected]
2002-11-04
Atzmon Ofri
Bonding Si to Si
Josef Kouba
2002-11-04
Hi Kenneth,

Thanks for your mail, I've received really lot of useful information
from many MEMS users and I appreciate each answer. At the moment, I'm
about to read all the papers I got and to sort out information I need. I
would appreciate any contacts you can give me about this topic.

Best regards

J.Kouba



-----Original Message-----
From: [email protected] [mailto:[email protected]]
On Behalf Of Kenneth Smith
Sent: Friday, November 01, 2002 1:52 PM
To: [email protected]
Subject: Re: [mems-talk] Bonding Si to Si


Jeff, The burden is yours, not the forums- there is a delete key on your

computer - last time I checked mine... as this topic that is relavent to

many MEMS users and research entities and better to ask the  voice of
experience rather than fall to the prey of those that think they know.

Josef,
I have a contact that you can call about this- he has current experience

with both anodic  ( no oxide) and fusion ( with Si02) . The process to
set either solution up is quite cost effective and simple with the right

tools.

Regards,
Ken Smith

Jeff Birkmeyer wrote:

> Josef,
>
> Why don't you try a google search before you burden this forum with
> questions like this.  There is a ton of info on this out there.
>
> Regards,
>
> Jeff
>
> -----Original Message-----
> From: Josef Kouba [mailto:[email protected]]
> Sent: Thursday, October 31, 2002 11:18 AM
> To: 'MEMS talk'
> Subject: [mems-talk] Bonding Si to Si
>
>
> Hi all MEMS talk members,
>
> can anybody give me some advise how to bond two silicon wafers
> together? Do I need some special wafers for it or can I use common
> wafers? I would also appreciate any reliable and good information
> source about this problem.
>
> Thanks for your help
>
> Best Regards
>
> Josef Kouba
> Louisiana State University
> Center foot Advanced Microstructures & Devices
> 6980 Jefferson Hwy.
> Baton Rouge, LA 70806, USA
> (225) 578-9371 - Tel.
> (225) 578-6954 - Fax.
>
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list

> options, visit http://www.memsnet.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list

> options, visit http://www.memsnet.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/
>
>


--


Kmbh Associates
47 Rocket Circle
Rancho Cordova, CA 95742  U  S  A
510-714-5055 Efax- 510 217 4421 or 561 658 6136

High Purity Float Zone and Specialty CZ Silicon  for Power, IR and
Mirror Optics, Optoelectronics, MEMS, SOI, and other Semiconductor
applications. Service in SOI, Polishing SSP and DSP.
Quartz, Glass, Pyrex and Borofloat Wafer Supply. Anodic Bonding. SOG,
SOS.



_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://www.memsnet.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
MEMS Technology Review
University Wafer