A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: How to make PDMS more hydrophobic?
How to make PDMS more hydrophobic?
2002-12-09
Xinyu Li
2002-12-10
Bill Moffat
How to make PDMS more hydrophobic?
Bill Moffat
2002-12-10
Xinyu,
      Any vacuum vapor prime with a good silane such as HMDS will make a surface
hydrophobic.  Contact me and I will walk you through any problems.  Bill Moffat.

-----Original Message-----
From: Xinyu Li [mailto:[email protected]]
Sent: Monday, December 09, 2002 8:38 AM
To: [email protected]
Subject: [mems-talk] How to make PDMS more hydrophobic?


Dear colleagues,

Do you know how to make PDMS more hydrophobic?

Thanks.

Xinyu Li


_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
The Branford Group
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing