Kapton holes cutting
2002-12-10
lucia beccai
2002-12-13
Robert Dean
2002-12-12
Michael D Martin
2002-12-12
Maurice Norcott
2002-12-12
Alex Pozdin
Kapton holes cutting
lucia beccai
2002-12-10
Dear all,

I'm searching information about the different technical possibilities to
cut holes of 200 micron diameter in Kapton film.
The profile of the material must keep a good quality.

Any input is appreciated.
Regards,
Lucia Beccai



--
----------------------------------------------
Lucia Beccai
CRIM Lab
Polo Sant'Anna Valdera
Scuola Superiore Sant'Anna
Viale Rinaldo Piaggio 34 - 56025 -Pontedera (Pisa) - Italy
phone: +39 050 883 488
fax  +39 050 883 402
http://www-crim.sssup.it/



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
The Branford Group