MEMSnet Home: MEMS-Talk: Copper CMP
Copper CMP
2003-01-09
josh wo
2003-01-09
bille@npphotonics (Bill Eaton)
Copper CMP
bille@npphotonics (Bill Eaton)
2003-01-09
Rodel (www.rodel.com) and Cabot (www.cabotcmp.com) are two of the biggest
players in CMP. Both companies sell pads and slurries.

There's a smaller company in the Northeast, Universal Photonics
(www.universalphotonics.com) that definitely makes pads, but it's unclear
what their product is for copper polish slurries.

Regards,

Bill Eaton, Ph.D.
Materials & Analysis Manager
NP Photonics
5706 Corsa Avenue, Suite 100
Westlake Village, CA  91362
Voice:  (818) 991-7044 x211
eFax:   (503) 214-5559
mailto://[email protected]

> -----Original Message-----
> From: [email protected]
> [mailto:[email protected]]On Behalf Of josh wo
> Sent: Thursday, January 09, 2003 8:39 AM
> To: [email protected]
> Subject: [mems-talk] Copper CMP
>
>
>
> Dear Experts,
> I am trying to develop a Copper CMP process using thoe PM5
> polisher that made by Logitech. Unfortunately I can't get any
> infor from them because I bought a used machine from else
> where. So, I was hoping if any one can point me to the right
> direction ......things like where to get the slurries or
> chemicals ......
>
> Thank you very much
> Josh
> --
> __________________________________________________________
> Sign-up for your own FREE Personalized E-mail at Mail.com
> http://www.mail.com/?sr=signup
>
> Meet Singles
> http://corp.mail.com/lavalife
>
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
University Wafer
Tanner EDA by Mentor Graphics