MEMSnet Home: MEMS-Talk: selective etchant for SiN/InGaAs
selective etchant for SiN/InGaAs
2003-01-24
Wei Wei
selective etchant for SiN/InGaAs
Wei Wei
2003-01-24
Dear all;

I need an etxhant that will etch SiN and do not attack InGaAs.

If you have any ideas, please let me know!

Thanks,

W.