MEMSnet Home: MEMS-Talk: nickel as a mask in EDP
nickel as a mask in EDP
2003-02-03
Prem Pal
2003-02-03
Dan.W.Chilcott
2003-02-03
[email protected]
2003-02-04
[email protected]
nickel as a mask in EDP
[email protected]
2003-02-03
> -----Original Message-----
> From: Prem Pal [mailto:[email protected]]
> Sent: Monday, February 03, 2003 3:48 AM
> To: [email protected]
> Subject: [mems-talk] nickel as a mask in EDP
>
>
> Dear all
> Can electroless or electroplated Nickel be used as a mask for
> anisotropic etching in EDP.any type of suggetion would be highly
> appreciated.
> thanx

In our tests, evaporated nickel (with a chromium adhesion layer)
was not etched at all in KOH. EDP tends to be a little less aggressive
and probably will not etch the nickel, either.

        --Kirt Williams Agilent Technologies

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
MEMS Technology Review
Addison Engineering