Etching rate for BCB
2003-02-05
haixinzhu
2003-02-06
Lester Lopez
2003-02-10
Zhang Zhenfeng
2003-02-06
Bill Moffat
2003-02-10
Ivan Shubin
Etching rate for BCB
Lester Lopez
2003-02-06
Michael,

It all depends on the recipe that you are using.  At 500 uTorr and 300
Watts I've experienced plasma etch rates greater than 1.25 um per
minute.

Lester Lopez
Research Assistant
Wireless and Microwave Research Group
Department of Electrical Engineering
University of South Florida
4202 E. Fowler Ave ENB 118
Tampa, FL 33620
Tel: 813-974-4851
Fax: 813-974-5250
[email protected]


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Addison Engineering
MEMS Technology Review
Process Variations in Microsystems Manufacturing