dry etch indium oxides and tin oxides
2003-02-25
Andre Wong
2003-02-26
[email protected]
2003-02-27
Michael Yakimov
dry etch indium oxides and tin oxides
Michael Yakimov
2003-02-27
ITO and it's etch by-products are relatively high vapor pressure materials..
you may want to check with the person responsible for the tool about
cross-contamination issues before even trying to find etch process..
Mike



> -----Original Message-----
> From: [email protected]
> [SMTP:[email protected]]
> Sent: Wednesday, February 26, 2003 10:35
> To:   [email protected]
> Subject:      [mems-talk] dry etch indium oxides and tin oxides
>
>
> Andre
>
> What system do you have to etch these materials?  Without that info it
> will
> be difficult to advise you.
>
> Richard
>
>
> Richard Barnett BEng(Hons) MIEE
> Product Marketing Engineer (MEMS)
>
>
>
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Process Variations in Microsystems Manufacturing
Addison Engineering
Tanner EDA by Mentor Graphics