A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: pyrex 7740
pyrex 7740
2003-03-19
Ravi Shankar
2003-03-19
Jesse Moreland
2003-03-19
sp
2003-03-19
Susan Coder
pyrex 7740
Jesse Moreland
2003-03-19
Hi Ravi,

I believe our company can help with your request.  We can supply and machine
polished glass wafers as well as other hard, brittle materials.  Please
contact me with your requirements or visit our website at
www.bullen-ultrasonics.com for more information.

Regards,

Jesse Moreland
Customer Service Manager
Bullen Ultrasonics Inc.
Ph. (937) 456-7521
Fx. (937) 456-2779
E-mail: [email protected]

-----Original Message-----
From:   [email protected] [mailto:[email protected]]
On Behalf Of Ravi Shankar
Sent:   Wednesday, March 19, 2003 7:15 AM
To:     [email protected]
Subject:        [mems-talk] pyrex 7740

could anyone tell me the rough estimate of price of 6" pyrex glass wafer
with holes drilled in them.
Regds
Ravi Shankar
India


_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Addison Engineering
Mentor Graphics Corporation
The Branford Group