Dear all,

Can I use SU-8 as a mask for ion exchange process. A typical ion exchange
process requires the sample (either silicon or quartz) to be immersed in a
silver nitrate (AgNO3) + sodium hydroxide (NaOH) mixture at a temp of 300C
for 1 - 2 hrs.

abang annuar