MEMSnet Home: MEMS-Talk: Etch through pyrex
Etch through pyrex
2003-04-11
Helen Berney
2003-04-11
[email protected]
2003-04-14
Dlee Li
Etch through pyrex
Helen Berney
2003-04-11
I am looking for someone who can etch through pyrex in a cmos compatible
way. Is this possible?

Helen.

Dr Helen Berney, MIEEE, MEBF
NMRC, Prospect Row, Cork, Ireland
Tel +353-21-4904010  Fax +353-21-4270271   Email [email protected]
http://www.nmrc.ie/research/transducers-group/index.html