cleaving of ultra-thin Si wafers
2003-04-15
Esteban Broitman
2003-04-16
Kenneth Smith
2003-04-17
Mario Robles
2003-04-21
Michael Barger
Photoresist.
2003-04-21
krishna
2003-04-21
Kenneth Smith
2003-04-17
Michael Yakimov
2003-04-18
[email protected]
2003-04-22
Tan Joo Lett
Photoresist.
krishna
2003-04-21
Dear all, I am trying to do electroplating of gold on silicon substrate covered
with thin layer of gold and photoresist on top of it.The Photoresist is opened
in some areas and i want to deposit gold in those areas. But after going for
some electrodepostion all i could observe that the plated areas are reddish
brown in colour instead of golden yellow colour and the plating is not following
the proper pattern and the photoresist is appeared to be disturbed and lifted
off and i could observe cracks in the photoresist. Please suggest me regarding
this problem. Thankskris




---------------------------------
Do you Yahoo!?
The New Yahoo! Search - Faster. Easier. Bingo.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
MEMS Technology Review
MEMStaff Inc.
Process Variations in Microsystems Manufacturing