Ucla Uses Nano-device To Find Cancer Cells

Technique uses sight and touch refined down to the cellular level to detect cancer

Nanoscientists at UCLA use an atomic force microscope to measure softness. The probe is the size of 30 atoms.

Posted: 2008-03-14