Material: Aluminum Nitride (AlN), bulk

To purchase MEMS-related materials, supplies, equipment, wafers, etc.,please visit the links section of the MEMSNet site.

Property↑↓Value↑↓Conditions↑↓Reference↑↓
Density3260 .. 3300 kg/m^3CeramicCRC Materials Science and Engineering Handbook, p.50
Electrical resistivity0.02 .. 1e+11 Ω*mCeramic,at room temperatureCRC Materials Science and Engineering Handbook, p.564
Hardness,Knoop(KH)1225 .. 1230 kg/mm/mm100g,CeramicCRC Materials Science and Engineering Handbook, p.472
Heat capacity819.7 J/kg/KAt temp=0-100 C.CRC Materials Science and Engineering Handbook, p.263
Heat capacity951.79 J/kg/KAt temp=0-420 C.CRC Materials Science and Engineering Handbook, p.263
Heat capacity1002.78 J/kg/KAt temp=0-598 C.CRC Materials Science and Engineering Handbook, p.263
Modulus of Rupture2624.5 GPaCeramic,at temp=1400 CCRC Materials Science and Engineering Handbook, p.533
Modulus of Rupture0.2655 GPaCeramic,hot pressed,at temp=25 CCRC Materials Science and Engineering Handbook, p.533
Modulus of Rupture0.1862 GPaCeramic, at temp=1000 CCRC Materials Science and Engineering Handbook, p.533
Thermal conductivity30.1 W/m/KCeramic,at temp=25 C.CRC Materials Science and Engineering Handbook, p.280
Thermal conductivity22.15 W/m/KCeramic,at temp=400 C.CRC Materials Science and Engineering Handbook, p.280
Thermal conductivity20.06 W/m/KCeramic,at temp=600 C.CRC Materials Science and Engineering Handbook, p.280
Young's Modulus344.83 GPaCeramic,at temp=25 CCRC Materials Science and Engineering Handbook, p.508
Young's Modulus317.24 GPaCeramic,at temp=1000 CCRC Materials Science and Engineering Handbook, p.508
Young's Modulus275.86 GPaCeramic,at temp=1400 CCRC Materials Science and Engineering Handbook, p.508