Property↑↓Value↑↓Conditions↑↓Reference↑↓
Compressive strength4.138 GPaCeramicCRC Materials Science and Engineering Handbook, p.419
Density6700 kg/m^3CeramicCRC Materials Science and Engineering Handbook, p.50
Hardness,Knoop(KH) or Vickers(VH)1019 .. 1834 kg/mm/mmCeramicCRC Materials Science and Engineering Handbook, p.472
Thermal conductivity189.77 W/m/KCeramicCRC Materials Science and Engineering Handbook, p.279
Young's Modulus373.13 GPaCeramicCRC Materials Science and Engineering Handbook, p.508