Property↑↓Value↑↓Conditions↑↓Reference↑↓
Hardness,Vickers(VH)1120 .. 1230 kg/mm/mm500g,Ceramic,1010 face,10um diagonalCRC Materials Science and Engineering Handbook, p.474
Hardness,Vickers(VH)1040 .. 1130 kg/mm/mm500g,Ceramic,1011 face,10um diagonalCRC Materials Science and Engineering Handbook, p.474
Hardness,Vickers(VH)1300 kg/mm/mm500g,Ceramic,polished 1010 face,10um diagonalCRC Materials Science and Engineering Handbook, p.475