Property↑↓Value↑↓Conditions↑↓Reference↑↓
Compressive strength0.006897 .. 0.06897 GPaCeramic at temp=25 CCRC Materials Science and Engineering Handbook, p.419
Compressive strength0.06897 .. 0.2069 GPaCeramic at temp=1000 CCRC Materials Science and Engineering Handbook, p.419
Hardness,Knoop(KH) or Vickers(VH)815 .. 1936 kg/mm/mmCeramicCRC Materials Science and Engineering Handbook, p.473
Heat capacity710.6 J/kg/K-CRC Materials Science and Engineering Handbook, p.263