Material: Sillimanite (Al2O3 SiO2), bulk

To purchase MEMS-related materials, supplies, equipment, wafers, etc.,please visit the links section of the MEMSNet site.

Property↑↓Value↑↓Conditions↑↓Reference↑↓
Density3230 .. 3240 kg/m^3CeramicCRC Materials Science and Engineering Handbook, p.50-52
Thermal conductivity1.76 W/m/KCeramic,at temp=100 C,porosity=0%.CRC Materials Science and Engineering Handbook, p.287
Thermal conductivity1.67 W/m/KCeramic,at temp=400 C,porosity=0%.CRC Materials Science and Engineering Handbook, p.287
Thermal conductivity1.46 W/m/KCeramic,at temp=800 C,porosity=0%.CRC Materials Science and Engineering Handbook, p.287
Thermal conductivity1.46 W/m/KCeramic,at temp=1200 C,porosity=0%.CRC Materials Science and Engineering Handbook, p.287
Thermal conductivity1.25 W/m/KCeramic,at temp=1500 C,porosity=0%.CRC Materials Science and Engineering Handbook, p.287