Material: Titanium Aluminum (Ti3Al), bulk

To purchase MEMS-related materials, supplies, equipment, wafers, etc.,please visit the links section of the MEMSNet site.

Property↑↓Value↑↓Conditions↑↓Reference↑↓
Young's Modulus110 .. 145 GPaBulk material.Thin Solid Films,270(1995), p.263