Material: Titanium Nitride (TiN), bulk

To purchase MEMS-related materials, supplies, equipment, wafers, etc.,please visit the links section of the MEMSNet site.

Property↑↓Value↑↓Conditions↑↓Reference↑↓
Compressive strength0.9724 GPaCeramicCRC Materials Science and Engineering Handbook, p.419
Density5430 kg/m^3CeramicCRC Materials Science and Engineering Handbook, p.50-52
Electrical resistivity11.07 .. 1.3e+06 Ω*mCeramic,at room temperatureCRC Materials Science and Engineering Handbook, p.565
Electrical resistivity3.4e+06 Ω*mCeramic,at melting temperatureCRC Materials Science and Engineering Handbook, p.565
Electrical resistivity81300 Ω*mCeramic,at liquid air temperatureCRC Materials Science and Engineering Handbook, p.565
Hardness,Knoop(KH)2160 kg/mm/mm30g,CeramicCRC Materials Science and Engineering Handbook, p.472
Hardness,Knoop(KH)1770 kg/mm/mm100g,CeramicCRC Materials Science and Engineering Handbook, p.472
Modulus of Rupture4930 GPaCeramicCRC Materials Science and Engineering Handbook, p.534
Thermal conductivity28.84 W/m/KCeramic,at temp=25 C.CRC Materials Science and Engineering Handbook, p.281
Thermal conductivity23.83 W/m/KCeramic,at temp=127 C.CRC Materials Science and Engineering Handbook, p.281
Thermal conductivity16.72 W/m/KCeramic,at temp=200 C.CRC Materials Science and Engineering Handbook, p.281
Thermal conductivity11.29 W/m/KCeramic,at temp=650 C.CRC Materials Science and Engineering Handbook, p.281
Thermal conductivity8.36 W/m/KCeramic,at temp=1000 C.CRC Materials Science and Engineering Handbook, p.281
Thermal conductivity67.72 W/m/KCeramic,at temp=1500 C.CRC Materials Science and Engineering Handbook, p.281
Thermal conductivity56.85 W/m/KCeramic,at temp=2300 C.CRC Materials Science and Engineering Handbook, p.281
Young's Modulus79.096 .. 250.37 GPaCeramicCRC Materials Science and Engineering Handbook, p.509