Property↑↓Value↑↓Conditions↑↓Reference↑↓
Dielectric constant,relative9.9 .. 11Bulk values reported in the literature.IEEE Micro Electro Mechanical Systems Workshop,Jan-Feb 1991,Nara, Japan, p.118
Piezoelectric coefficient12.4 pC/NBulk values reported in the literature.IEEE Micro Electro Mechanical Systems Workshop,Jan-Feb 1991,Nara, Japan, p.118
Young's Modulus12 .. 201000 GPaBulk values reported in the literature.IEEE Micro Electro Mechanical Systems Workshop,Jan-Feb 1991,Nara, Japan, p.118