Dear colleagues,

Is anyone can tell me how to etch trace Nickel from the surface of copper? I
used a commercialised etchant (), but I found trace nickel was left which
rendered the copper surface look black. any ideas of removing the black surface
to achieve a nice copper surface (without attacting copper) are wecome.

Many thanks

James