MEMSnet Home: MEMS-Talk: Methanol as lubricant for PDMS alignment/bonding
Methanol as lubricant for PDMS alignment/bonding
2006-03-02
[email protected]
2006-03-03
[email protected]
2006-03-04
[email protected]
Methanol as lubricant for PDMS alignment/bonding
[email protected]
2006-03-04
Thank you for sharing your experiences, Joe. What you described was actually
quite similar to the cases that I've met.
I've recently tried "1 or 2 drops of methanol" on PDMS which has a surface
area of about 2 or 3 cm^2. Using few methanol makes it slightly better, I
mean bonding,  than using more methanol, but still not as good as other
people reported.
I'll try your suggestions soon. THanks
--
Best Regards,
Yu Xiang
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
University Wafer
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing