MEMSnet Home: MEMS-Talk: Problem in etching buried oxide
Problem in etching buried oxide
2006-05-02
Julie Verstraeten
2006-05-02
David Nemeth
2006-05-04
ZICKAR Michaël
2006-05-05
walter essinger
2006-05-02
Beggans Michael H IHMD
2006-05-18
Mandar Deshpande
2006-05-26
Micro Sense
2006-05-27
Micro Sense
Problem in etching buried oxide
ZICKAR Michaël
2006-05-04
Hi,

After cleaning your wafer by a O2 plasma or pyranha you could do a vapor HF
etching of the buried SiO2. The problem with liquid HF etching is that it is
difficult to fill deep holes with the etchant. This is not the case for vapor
HF. If you want we could do a test etching for you.

Best regards,

Michael
idonus.com

________________________________

Von: [email protected] im Auftrag von Julie Verstraeten
Gesendet: Di 02.05.2006 17:28
An: General MEMS discussion
Betreff: [mems-talk] Problem in etching buried oxide




Hi,


I need to etch holes through SOI wafer (for front/back alignment). The holes
have a diameter of 200 microns.

The procedure is as follow:

- first of all I deep etch (DRIE) the holes through the device layer (30 microns
thick) until I reach the buried oxide,

- then I wet etch the oxide layer (10 microns thick), in the bottom of the
etched holes (BOE),

- at last I etch the holes (DRIE) through the handle layer (400 microns thick).


The problem is that the buried oxide doesn't etch well.

In the first 1 hour nothing happens as if there was a protective layer above the
oxide. The etching of the handle layer however finishes by an etching period
and there's no C4F8 plasma during this period to avoid passivating the buried
oxide.

After 1 hour it begins to etch (2-3 microns in two hours - BOE at 30°C, the
liquid is magnetically agitated).

After these 3 hours etching I started again 2 hours and nothing was etched.

I don't know the nature of the buried oxide.

Has anyone ever had the problem?

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
MEMS Technology Review
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing