Ammonium fluoride
Gareth Jenkins
2006-05-10
Hi Paul

If I remember correctly it is approximately 0.1 um /min depending on how
fresh the solution is.

Paul Monaghan wrote:

>Gareth,
>
>out of interest, what sort of etch rates do you get for sodalime glass with
>that etchant?
>
>thanks,
>
>Paul
>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Tanner EDA by Mentor Graphics
MEMS Technology Review
Process Variations in Microsystems Manufacturing