MEMSnet Home: MEMS-Talk: Help needed for PMMA Exposure
Help needed for PMMA Exposure
2006-05-30
Abhay Kulkarni
2006-05-31
[email protected]
2006-05-31
Abhay Kulkarni
Help needed for PMMA Exposure
Abhay Kulkarni
2006-05-31
Thanks for the correction Dr. Friedrich, PMMA thickness is 5-8 microns.

Regards,
Abhay


On 5/30/06, [email protected]  wrote:
>
> you mis-typed the thickness....you have 5-8mm which requires x-ray.  You
> meant 5-8 um.
>