MEMSnet Home: MEMS-Talk: sealing cavity in capacitive pressure sensor
sealing cavity in capacitive pressure sensor
2009-01-24
Reza Rashidi
2009-01-24
Brad Cantos
2009-01-25
Ulli Hansen - MSG Lithoglas AG
2009-01-25
Reza Rashidi
2009-01-26
shay kaplan
sealing cavity in capacitive pressure sensor
shay kaplan
2009-01-26
Resa

I'm not at the office but a search for microspheres should get you there

Shay

-----Original Message-----
From: [email protected] [mailto:[email protected]]
On Behalf Of Reza Rashidi
Sent: Sunday, January 25, 2009 10:21 PM
To: Brad Cantos; General MEMS discussion
Subject: Re: [mems-talk] sealing cavity in capacitive pressure sensor

Hi Brad,

Thank you very much for your explanation. Just I searched precision glass
sphere or bead, but I couldn't find a proper supplier. Do you know one to
introduce it to me? Also, I used frit tape instead of paste. Do you think if
I use glass frit paste it flows to the cavity due to high pressure and
temperature?

Best regards,
Reza


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
MEMS Technology Review
Process Variations in Microsystems Manufacturing
Addison Engineering