Hi everyone
I am having 2 questions related to electroplating

1 Can I use like Counter and Reference Electrodes same Wire? (I am
just put the REF and Counter electrodes outputs of the potentiostat in
short and leave from there with only one wire which I am immersing in
electrolyte next to the workings )

2 I am plating Cobalt (From CoSulfamate and Boric Acid solution) using
a Co wire like reference and also like Counter electrode on a Au
working electrode . What potential should I use ?
Co2+ +2e  --->Co  -0.3 V (approx)

Any help with these?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
MEMS Technology Review