Roger Shile
2009-02-10
Pyrex is a borosilicate glass.  You can bond the Pyrex directly to the
silicon wafer without the need to deposit additional borosilicate glass.
In fact borosilicate isn't absolutely necessary for anodic bond.  Any
mobile ion containing glass should work.

Roger Shile

-----Original Message-----
Hi everyone,

I am going to evaporate or sputter a kind of Borosilicate glass (or
similar) on pyrex to anodically bond pyrex to si wafer. Does anyone
knows where I can buy some sample of the glass for evaporation or
sputtering?

Any help will be highly appreciated.

Thanks,
Reza Rashidi

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics
Addison Engineering