Storage of developed AZ photoresist
2009-07-10
Y.Tian
2009-07-13
Krueger, Bernd
2009-07-13
Y.Tian
2009-07-13
Krueger, Bernd
2009-07-13
Y.Tian
2009-07-15
Krueger, Bernd
Storage of developed AZ photoresist
Y.Tian
2009-07-10
Hi All,

Does anybody have the experience about storage of the wafers with developed AZ
photoresist patterns? I just got loads of samples patterned with AZ, but I can
not use them immediately. I just have general idea that I should keep them away
from UV and keep them dry. Anything specific I should keep in mind?

Thank you all.

Yingtao
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
MEMS Technology Review